MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® HB 5299 HV PA*
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, suitable for blown film- and extrusion blow molding applications.
  • Excellent oxygen and carbon dioxide barrier, especially in interaction with moisture (50 up to 100% relative humidity)
  • Excellent transparency, even for thicker Components
  • Suitable as a middle layer in multi-layer films and components
  • Suitable for co-extruded and oriented multilayer films in conjunction with all polyamides, polyesters and polyolefins
  • Barrier properties are hardly affected by steam sterilization. Transparency depends on layer structure and other polymers used.
Application: Grivory HB 5299 HV is used in various multi layer structures providing high barrier (oxygen, carbon dioxide, nitrogen, …) e.g. Co-extruded blown films and EBM containers

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccDry; ISO 1183
Water Absorption 5.5 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Water Vapor Transmission 6.00 g/m²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 30 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 4.5 %ISO 527-3
Film Elongation at Break, TD 3.5 %ISO 527-3
Tensile Modulus 4000 MPaDry; ISO 527-1/-2
Film Tensile Strength at Break, MD 110 MPaISO 527-3
Film Tensile Strength at Break, TD 100 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 218 °C10°C/min; ISO 11357-1/-3
 
Optical PropertiesOriginal ValueComments
Gloss 150 %60°; ISO 2813
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)15ISO 15105-1/-2; 23°C/0% RH
 15ISO 15105-1/-2; 23°C/ 85% RH
Elmendorf Tear Resistance, Normal (N)5ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)5ISO 6383-2
Food contactEU Requirements
FormGranules
Oxygen Transmission Rate, cm³/(m²*d*bar)4ISO 15105-1/-2; 23°C/0% RH
 4ISO 15105-1/-2; 23°C/ 85% RH
PackagingBlow molded containers
 Injection, stretch, blow molded containers
 Medical packaging
 Non oriented film
 Oriented film
 Paper coating
 Tubes
ProcessingBlown Film Extrusion
 Extrusion - blow molding
 Film Extrusion
 Other Extrusion
Product AttributesBarrier Properties
 High viscosity
 Partially aromatic Polyamide
 Transparent Polyamide
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® 833C Nylon 66, Extrusion Grade
Ascend Performance Materials Vydyne® 833F Nylon 66, Extrusion Grade
Domo Domamid® 33 Polyamide 6
Envalior Akulon® F130-C2 PA6
Envalior Novamid® 2620A PA6/6T

PGRH363 / 157072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.