MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik Sanicro 53 Welding wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sanicro 53 is a nickel-chrome-cobalt-molybdenum alloy of type alloy 617. It has an excellent resistance to high temperature corrosion such as oxidation and carburization. The weld metal provides a combination of excellent metallurgical stability and strength in short and long term exposure to temperatures up to 1100°C (2012°F). Applications for Sanicro 53 are found in high temperature heat exchangers and valves, furnace tubing in the petrochemical industry, radiant heat tubes, gas turbines, components subjected to high temperatures in the chemical processing industry and components for power plants. Sanicro 53 is suitable for joining heat resistant nickel alloys, heat resistant austenitic and cast alloys such as:
  • UNS N08810 (1.4958)
  • UNS N08811 (1.4959)
  • UNS N06617 (2.4663)
Sanicro 53 can also be used for surfacing.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 260260
Tensile Strength, Ultimate 770 MPa112000 psi
Tensile Strength, Yield 510 MPa
@Strain 0.2 %
74000 psi
@Strain 0.2 %
Elongation at Break 37 %37 %
Reduction of Area 42 %42 %
Charpy Impact  105 J
@Temperature -196 °C
77.4 ft-lb
@Temperature -321 °F
 130 J
@Temperature 20.0 °C
95.9 ft-lb
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.0 %1.0 %Filler metal
Carbon, C 0.060 %0.060 %All-weld metal
 0.080 %0.080 %Filler metal
Chromium, Cr 22.5 %22.5 %Filler metal
 22.5 %22.5 %All-weld metal
Cobalt, Co 11.5 %11.5 %All-weld metal
 12 %12 %Filler metal
Iron, Fe 0.50 %0.50 %All-weld metal
 <= 1.0 %<= 1.0 %Filler metal
Manganese, Mn 0.040 %0.040 %All-weld metal
 <= 1.0 %<= 1.0 %Filler metal
Molybdenum, Mo 9.0 %9.0 %Filler metal
 9.0 %9.0 %All-weld metal
Nickel, Ni 53.5 %53.5 %Filler metal
 55 %55 %All-weld metal
Phosphorus, P <= 0.010 %<= 0.010 %Filler metal
Silicon, Si 0.20 %0.20 %All-weld metal
 <= 1.0 %<= 1.0 %Filler metal
Sulfur, S <= 0.010 %<= 0.010 %Filler metal
Titanium, Ti <= 0.60 %<= 0.60 %Filler metal
Tungsten, W <= 0.10 %<= 0.10 %All-weld metal
 <= 0.50 %<= 0.50 %Filler metal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 617
Industeel SIRIUS 800 H+ Heat Resistant Alloy

NSANDV5255 / 199819

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.