MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akro-Plastic Akromid® A3 1 L black (4652) PA 66 + PP Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced; Polypropylene (PP)

Material Notes: Description: Akromid A3 L 1 black (4652) is a nonreinforced and heat stabilized polyamide-blend with a reduced density compared to standard PA66. Applications are mainly technical components in the automotive and electronic industry, where a weight and cost reduction is required.

Features:

  • Heat Stabilized
  • Low Density
Uses:
  • Automotive Applications
  • Electrical/Electronic Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption at Saturation 1.7 %1.7 %ISO 62
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4
Melt Flow 29 g/10 min
@Load 5.00 kg,
Temperature 275 °C
29 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Spiral Flow 105 cm41.3 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psi50 [mm/min]; ISO 527-2
Elongation at Break 30 %30 %50 [mm/min]; ISO 527-2
Tensile Modulus 2.30 GPa334 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDSC, 10K/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75-2/A
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Glow Wire Ignition Temperature 800 °C
@Thickness 0.800 mm
1470 °F
@Thickness 0.0315 in
IEC 60695-2-13
Glow Wire Flammability Index 775 °C
@Thickness 0.800 mm
1430 °F
@Thickness 0.0315 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 270 - 290 °C518 - 554 °F
Zone 1 230 - 295 °C446 - 563 °F
Zone 2 230 - 295 °C446 - 563 °F
Zone 3 230 - 295 °C446 - 563 °F
Zone 4 230 - 295 °C446 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time <= 2.00 hour<= 2.00 hour
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 5.00 MPa725 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8253 HS PA6 (Dry)
Overview of materials for Polypropylene, Molded
Abatron AboCast 50-3/AboCure 50-12 Epoxy
Amco PRIMATOP PP HOMO 200NA Homopolymer Polypropylene
Chevron Phillips EA3025 Crystal Polystyrene

PAKRO111 / 182698

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.