MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2599 X 131264 B Polycarbonate/ABS Alloy (PC/ABS), Carbon Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive; Polycarbonate (PC)

Material Notes: Preliminary Data Sheet

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10500 psiASTM D 638
Elongation at Break 1.0 %ASTM D 638
Tensile Modulus 1000 ksiASTM D 638
Flexural Strength 16000 psiASTM D 790
Flexural Modulus 1000 ksiASTM D 790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 7.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 72 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 72 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 74 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 75 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 77 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 79 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 525 °F
Mold Temperature 125 - 200 °F
Drying Temperature 200 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 2585 Polycarbonate/ABS Alloy (PC/ABS), Carbon Fiber
RTP Company RTP 2583 Polycarbonate/ABS Alloy (PC/ABS), Carbon Fiber
RTP Company RTP 2581 Polycarbonate/ABS Alloy (PC/ABS), Carbon Fiber

PQZTA25161 / 159249

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.