MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax 6323 Polypropylene Homopolymer, Easy Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: General Purpose

Key Features: easy molding, FDA acceptable, general purpose polypropylene homopolymer resin

Applications: containers, closures, hospital and institutional ware, toys

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax 6323 resin is a general purpose polypropylene homopolymer. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI. These UL ratings apply only to natural color resin. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792B
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 88ASTM D785A
Tensile Strength, Yield 34.0 MPaASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus, 1% Secant 1.40 GPa0.05 in/min; ASTM D790A
Izod Impact, Notched 0.350 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
UL RTI, Mechanical with Impact 110 °C
@Thickness >=1.02 mm
Flammability, UL94 HB
@Thickness >=1.47 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
LyondellBasell Pro-fax 6331 Polypropylene Homopolymer, Easy Molding
Flint Hills P5M6K-048 Random Copolymer Polypropylene
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer

PMO009 / 53492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.