MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Proto3000 HP 3D High Reusability PA 12 3D Printing MultiJet Fusion Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: HP 3D High Reusability PA 12 is a robust thermoplastic that produces high-density parts with balanced property profiles and strong structures. This material was designed for the production of functional parts across a variety of industries such as watertight applications without any additional post-processing. HP 3D High Reusability PA 12, also known as Nylon PA12, is a thermoplastic material that produces high-density parts with balanced property profiles and strong structures. HP 3D High Reusability PA 12 provides good chemical resistance to oils, greases, aliphatic hydrocarbons, and alkalies and is the optimal material for complex assemblies, housings, enclosures, and watertight applications. Due to the surplus powder reusability, you can minimize the waste, thus achieving a low cost per part. Work with Proto3000’s ISO 9001:2015 quality certified manufacturing services to have parts made with HP Nylon 12.

Applications:

  • Rapid Prototyping-Prototypes and final parts.
  • Production Parts- Strong and durable end-use parts such as living hinges or snap fits
  • Consumer Goods and Electronics- Create customer-centric highly customized experiences
  • End of Arm Tooling- Lightweight tools customized for automation applications
  • Orthotics, Prosthetics, and Medical Devices- Build strong and high-customized devices for patient-specific results
  • Replacement Parts and Supply-Chain Fixes- Build parts when and where you need them, quickly and on-demand
Uses
  • Complex assemblies
  • Housings
  • Enclosures & connectors
  • Watertight applications
  • Orthotics, prosthetics and medical devices
  • End-of-arm tooling, robotics and automation
Industries
  • Industrial goods
  • Consumer goods
  • Healthcare
  • Education
  • Aerospace
  • Transportation and Automotive
Certifications: USP Class I-VI and US FDA guidance for Intact Skin Surface Devices, RoHS, EU REACH, PAHs

Information provided by Proto3000

Key Words: MJF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.425 g/cc0.0154 lb/in³
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Particle Size 60.0 µm60.0 µmASTM D3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 48.0 MPa6960 psimax load, XY, 10 mm/min, specimens type V; ASTM D638
 48.0 MPa6960 psimax load, Z, 10 mm/min, specimens type V; ASTM D638
Elongation at Break 15.0 %15.0 %Z, 10 mm/min, specimens type V; ASTM D638
 20.0 %20.0 %XY, 10 mm/min, specimens type V; ASTM D638
Modulus of Elasticity 1.60 GPa232 ksi
Tensile Modulus 1.70 GPa247 ksiXY, 10 mm/min, specimens type V; ASTM D638
 1.80 GPa261 ksiZ, 10 mm/min, specimens type V; ASTM D638
Flexural Strength  65.0 MPa
@Strain 5.0 %
9430 psi
@Strain 5.0 %
XY, Procedure B at a test rate of 13.55 mm/min; ASTM D790
 70.0 MPa
@Strain 5.0 %
10200 psi
@Strain 5.0 %
Z, Procedure B at a test rate of 13.55 mm/min; ASTM D790
Flexural Modulus 1.73 GPa251 ksiProcedure B at a test rate of 13.55 mm/min; ASTM D790
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Thickness 3.20 mm
1.67 ft-lb/in²
@Thickness 0.126 in
ASTM D256 Test Method A
Charpy Impact, Notched 3.50 J/cm²16.7 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Melting Point 187 °C369 °FPowder; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FXY, Z; ASTM D648 Test Method A
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FXY; ASTM D648 Test Method A
 106 °C223 °FZ; ASTM D648 Test Method A
 
Descriptive Properties
Refresh ratio for stable performance (%)20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROTO800 / 322813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.