MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AGC Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Modified ETFE, Unreinforced

Material Notes: Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive agent or surface treatment that is used at previous system. Excellent adhesiveness of the two-layer system is effected for only one step. Furthermore, the conventional properties such as anti stick, excellent moldability and chemical resistance, are same as conventional fluoro-resin.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 g/ccASTM D792
Melt Flow 25 g/10 minASTM D359
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 49.0 MPaASTM D638
Elongation at Break 420 %ASTM D638
Flexural Modulus 0.790 GPaASTM D790
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °C
 
Descriptive Properties
Permeation Rate2.6 g-mm/m2-24hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® LM-740AP LM-ETFE Fluororesin
AGC Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin
AGC Fluon® LM-720AP LM-ETFE Fluororesin
AGC Fluon® LH-8000 ETFE
AGC Fluon® EA-2000 Perfluoro Adhesive

PAGC18 / 22977

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.