MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7776 Polypropylene Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adhesive 310, which is a firm adhesive which resists oozing and provides high strength on a variety of surfaces including high surface energy (HSE) plastics and metals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.3 microns0.800 milAdhesive
 66.0 microns2.60 milFacestock
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.07669 kN/m0.4375 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.0877 kN/m0.500 pliLD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.0877 kN/m0.500 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.09861 kN/m0.5625 pliHD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.1205 kN/m0.6875 pliPolypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.131 kN/m0.750 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.131 kN/m0.750 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.1424 kN/m0.8125 pliLD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.153 kN/m0.875 pliPolypropylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.153 kN/m0.875 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.1643 kN/m0.9375 pliHD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.175 kN/m1.00 pliPolypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.1972 kN/m1.125 pliLDPE, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.20817 kN/m1.1875 pliHDPE, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.20817 kN/m1.1875 pliPolycarbonate 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.23008 kN/m1.3125 pliHD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.23008 kN/m1.3125 pliLD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.23008 kN/m1.3125 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.2410 kN/m1.375 pliPolypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.25199 kN/m1.4375 pliLD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.27391 kN/m1.5625 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.27391 kN/m1.5625 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.27391 kN/m1.5625 pliHD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.2849 kN/m1.625 pliPolypropylene, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.3287 kN/m1.875 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.3725 kN/m2.125 pliGlass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.38347 kN/m2.1875 pliStainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.4163 kN/m2.375 pliStainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.4163 kN/m2.375 pliPolycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.44921 kN/m2.5625 pliGlass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.44921 kN/m2.5625 pliGlass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.49303 kN/m2.8125 pliGlass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.5040 kN/m2.875 pliPolycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.5040 kN/m2.875 pliStainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.526 kN/m3.00 pliPolycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.526 kN/m3.00 pliGlass, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.526 kN/m3.00 pliPolycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.53686 kN/m3.0625 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.53686 kN/m3.0625 pliStainless Steel, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
 0.5478 kN/m3.125 pliGlass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.5478 kN/m3.125 pliGlass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.5478 kN/m3.125 pliPolycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.58068 kN/m3.3125 pliStainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.58068 kN/m3.3125 pliPolycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.6793 kN/m3.875 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 79.0 °C174 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 10.0 °C>= 50.0 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type310 Acrylic
Liner55# Densified kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33736 / 168483

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.