Physical Properties | Metric | English | Comments |
---|
Density | 8.00 g/cc | 0.289 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell B | 96 | 96 |
Tensile Strength, Ultimate | 655 - 850 MPa @Diameter >=5.00 mm | 95000 - 123000 psi @Diameter >=0.197 in |
| 675 - 850 MPa @Diameter 5.00 mm | 97900 - 123000 psi @Diameter 0.197 in |
Tensile Strength, Yield | >= 310 MPa @Strain 0.2 % | >= 45000 psi @Strain 0.2 % |
| >= 340 MPa @Strain 1 % | >= 49300 psi @Strain 1 % |
| >= 148 MPa @Strain 0.2 %, Temperature 500 °C | >= 21500 psi @Strain 0.2 %, Temperature 932 °F |
| >= 160 MPa @Strain 0.2 %, Temperature 400 °C | >= 23200 psi @Strain 0.2 %, Temperature 752 °F |
| >= 170 MPa @Strain 0.2 %, Temperature 300 °C | >= 24700 psi @Strain 0.2 %, Temperature 572 °F |
| >= 180 MPa @Strain 1 %, Temperature 500 °C | >= 26100 psi @Strain 1 %, Temperature 932 °F |
| >= 190 MPa @Strain 1 %, Temperature 400 °C | >= 27600 psi @Strain 1 %, Temperature 752 °F |
| >= 190 MPa @Strain 0.2 %, Temperature 200 °C | >= 27600 psi @Strain 0.2 %, Temperature 392 °F |
| >= 200 MPa @Strain 1 %, Temperature 300 °C | >= 29000 psi @Strain 1 %, Temperature 572 °F |
| >= 225 MPa @Strain 1 %, Temperature 200 °C | >= 32600 psi @Strain 1 %, Temperature 392 °F |
| >= 230 MPa @Strain 0.2 %, Temperature 100 °C | >= 33400 psi @Strain 0.2 %, Temperature 212 °F |
| >= 270 MPa @Strain 1 %, Temperature 100 °C | >= 39200 psi @Strain 1 %, Temperature 212 °F |
Elongation at Break | >= 35 % | >= 35 % |
| >= 35 % @Thickness 50.8 mm | >= 35 % @Thickness 2.00 in |
Modulus of Elasticity | 195 GPa | 28300 ksi |
| 158 GPa @Temperature 500 °C | 22900 ksi @Temperature 932 °F |
| 166 GPa @Temperature 500 °C | 24100 ksi @Temperature 932 °F |
| 174 GPa @Temperature 300 °C | 25200 ksi @Temperature 572 °F |
| 182 GPa @Temperature 200 °C | 26400 ksi @Temperature 392 °F |
| 190 GPa @Temperature 100 °C | 27600 ksi @Temperature 212 °F |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 16.0 µm/m-°C @Temperature 30.0 - 100 °C | 8.89 µin/in-°F @Temperature 86.0 - 212 °F |
| 16.0 µm/m-°C @Temperature 30.0 - 200 °C | 8.89 µin/in-°F @Temperature 86.0 - 392 °F |
| 16.0 µm/m-°C @Temperature 30.0 - 100 °C | 8.89 µin/in-°F @Temperature 86.0 - 212 °F |
| 16.5 µm/m-°C @Temperature 30.0 - 300 °C | 9.17 µin/in-°F @Temperature 86.0 - 572 °F |
| 17.0 µm/m-°C @Temperature 30.0 - 500 °C | 9.44 µin/in-°F @Temperature 86.0 - 932 °F |
| 17.0 µm/m-°C @Temperature 30.0 - 500 °C | 9.44 µin/in-°F @Temperature 86.0 - 932 °F |
| 17.5 µm/m-°C @Temperature 30.0 - 700 °C | 9.72 µin/in-°F @Temperature 86.0 - 1290 °F |
| 17.5 µm/m-°C @Temperature 30.0 - 700 °C | 9.72 µin/in-°F @Temperature 86.0 - 1290 °F |
Specific Heat Capacity | 0.485 J/g-°C @Temperature 20.0 °C | 0.116 BTU/lb-°F @Temperature 68.0 °F |
| 0.510 J/g-°C @Temperature 100 °C | 0.122 BTU/lb-°F @Temperature 212 °F |
| 0.535 J/g-°C @Temperature 200 °C | 0.128 BTU/lb-°F @Temperature 392 °F |
| 0.565 J/g-°C @Temperature 300 °C | 0.135 BTU/lb-°F @Temperature 572 °F |
| 0.585 J/g-°C @Temperature 400 °C | 0.140 BTU/lb-°F @Temperature 752 °F |
| 0.600 J/g-°C @Temperature 500 °C | 0.143 BTU/lb-°F @Temperature 932 °F |
| 0.615 J/g-°C @Temperature 600 °C | 0.147 BTU/lb-°F @Temperature 1110 °F |
| 0.625 J/g-°C @Temperature 700 °C | 0.149 BTU/lb-°F @Temperature 1290 °F |
Thermal Conductivity | 10.0 W/m-K @Temperature 20.0 °C | 69.4 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
| 12.0 W/m-K @Temperature 100 °C | 83.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
| 14.0 W/m-K @Temperature 200 °C | 97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
| 16.0 W/m-K @Temperature 300 °C | 111 BTU-in/hr-ft²-°F @Temperature 572 °F |
| 18.0 W/m-K @Temperature 400 °C | 125 BTU-in/hr-ft²-°F @Temperature 752 °F |
| 20.0 W/m-K @Temperature 500 °C | 139 BTU-in/hr-ft²-°F @Temperature 932 °F |
| 21.0 W/m-K @Temperature 600 °C | 146 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| 23.0 W/m-K @Temperature 700 °C | 160 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Component Elements Properties | Metric | English | Comments |
---|
Carbon, C | <= 0.020 % | <= 0.020 % |
Chromium, Cr | 20 % | 20 % |
Copper, Cu | 0.70 % | 0.70 % |
Iron, Fe | 53.1 % | 53.1 % |
Manganese, Mn | <= 1.0 % | <= 1.0 % |
Molybdenum, Mo | 6.1 % | 6.1 % |
Nickel, Ni | 18 % | 18 % |
Nitrogen, N | 0.20 % | 0.20 % |
Phosphorus, P | <= 0.030 % | <= 0.030 % |
Silicon, Si | <= 0.80 % | <= 0.80 % |
Sulfur, S | <= 0.010 % | <= 0.010 % |