MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NuSil CV1-2640 Silicone, Conductive/Static Dissipative
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Two Part Adhesive and Sealant

Comments: Pumpable

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength at Break 3.62 MPa525 psi
Elongation at Break 225 %225 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 25 ohm-cm25 ohm-cm
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 150 g/min150 g/minB
 300 g/min300 g/minA
Cure Time 120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
 
Descriptive Properties
ColorBlack
Mix Ratio10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil CV3-2640 Silicone, Conductive/Static Dissipative
NuSil CV2-2644 Silicone, Conductive/Static Dissipative
NuSil CV2-2640 Silicone, Conductive/Static Dissipative

PNUSIL179 / 141903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.