MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Fastbond™ 4213-NF Industrial Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when dry. Neither prone to discolor with age nor stain substrates. Note: Not recommended for exterior applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 54 - 60 %54 - 60 %
Brookfield Viscosity 2500 - 5000 cP2500 - 5000 cPRVF #4 sp @ 20 rpm @ 62°C
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 3.45 MPa500 psiOverlap, Wood/Wood
 0.538 MPa
@Thickness 12800 mm,
Time 385000 sec
78.0 psi
@Thickness 504 in,
Time 107 hour
Overlap, 1/8" Birch/Birch
 0.600 MPa
@Thickness 12800 mm,
Time 335000 sec
87.0 psi
@Thickness 504 in,
Time 93.0 hour
Overlap, 1/8" Birch/Birch
 0.938 MPa
@Thickness 12800 mm,
Time 295000 sec
136 psi
@Thickness 504 in,
Time 82.0 hour
Overlap, 1/8" Birch/Birch
 1.24 MPa
@Thickness 12800 mm,
Time 238000 sec
180 psi
@Thickness 504 in,
Time 66.0 hour
Overlap, 1/8" Birch/Birch
 3.36 MPa
@Thickness 12800 mm,
Time 86400 sec
488 psi
@Thickness 504 in,
Time 24.0 hour
Overlap, 1/8" Birch/Birch
 5.13 MPa
@Thickness 12800 mm,
Time -133000 sec
744 psi
@Thickness 504 in,
Time -37.0 hour
Overlap, 1/8" Birch/Birch
Peel Strength  1.40 - 2.63 kN/m
@Temperature 24.0 °C,
Time 173000 sec
8.00 - 15.0 pli
@Temperature 75.2 °F,
Time 48.0 hour
180°, Supported Vinyl/Wood
 2.45 kN/m
@Temperature 82.0 °C,
Time 1.81e+6 sec
14.0 pli
@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
 2.63 kN/m
@Temperature -37.0 °C,
Time 1.81e+6 sec
15.0 pli
@Temperature -34.6 °F,
Time 504 hour
180°, Canvas/Steel
 2.63 kN/m
@Temperature 24.0 °C,
Time 86400 sec
15.0 pli
@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
 3.51 kN/m
@Temperature 66.0 °C,
Time 1.81e+6 sec
20.0 pli
@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
 4.21 kN/m
@Temperature 24.0 °C,
Time 259000 sec
24.0 pli
@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
 4.73 kN/m
@Temperature 24.0 °C,
Time 1.81e+6 sec
27.0 pli
@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
 5.26 kN/m
@Temperature 24.0 °C,
Time 432000 sec
30.0 pli
@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
 6.14 kN/m
@Temperature 24.0 °C,
Time 605000 sec
35.0 pli
@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
 6.14 kN/m
@Temperature 24.0 °C,
Time 1.21e+6 sec
35.0 pli
@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
 
Processing PropertiesMetricEnglishComments
Shelf Life 15.0 Month15.0 Month
 
Descriptive Properties
AppearanceWhite (Wet) Clear (Dry)
BaseSynthetic Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toho Tenax Tenax® HTA 5U41 Chopped Carbon Fiber
PTS PPE/Nylon Alloy 10% Glass Filled
LG Chemical DINP Plasticizer
Innospec VISCOWAX® 261 Oxidised PE-Wax
Cast Nylons Nycast® 6MPB Plasticized Nylon 6

PMM34044 / 168791

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.