MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibility, and low warpage. It contains skid additives. It is specially developed for lids fast-cycle molding injection, natural color and dyed for food. It is also used for oil and vinegar lids. IJ33D was developed to be injected in similar conditions to low-density polyethylene of similar fluidity. Recommended temperature profile: 150º to 210 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM-D729
ESCR 10% Igepal® 0.50 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM-D2240
Tensile Strength at Break 9.00 MPaASTM-D638
Tensile Strength, Yield 15.0 MPaASTM-D638
Elongation at Break 100 %ASTM-D638
Elongation at Yield 14 %ASTM-D638
Modulus of Rigidity 0.480 GPaASTM-D747
Flexural Modulus, 1% Secant 520 MPaASTM-D790
Izod Impact, Notched 90.0 J/mASTM-D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °CASTM-D648
Vicat Softening Point 97.0 °C
@Load 1.02 kg
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer
A. Schulman CP851 High Flow, Injection Molding Grade
A. Schulman CP814-01 Linear, Low-Density Polyethylene
Braskem IC32 LLDPE Injection Molding Polyethylene Copolymer
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer

PBRAS910 / 106756

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.