MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon® PTFE Grade 30B Aqueous Dispersion  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® PTFE 30B fluoropolymer resin is a negatively charged, hydrophobic colloid, containing approximately 60% (by total weight) of 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles suspended in water. Seen as a milky white liquid, it also contains approximately 8% (by weight of PTFE) of a nonionic wetting agent and stabilizer. Viscosity at room temperature is approximately 20 cP. Nominal pH is 10.

Compared with other grades of PTFE dispersions, Teflon® PTFE 30B is especially formulated to provide void-free coatings with enhanced surface smoothness and gloss. It imparts many of the unique properties of PTFE resin to porous structures. When properly processed, the PTFE resin in Teflon® PTFE 30B exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Teflon® PTFE 30B is used for coated glass fabric for high-performance industrial or food conveyor belting and nonadhesive separator sheets for laminating or press blankets requiring high-quality surface finish; electrical insulation for wire, printed circuit boards, and rotating equipment; cast film for capacitors or chemical barriers; and surface coatings for other substrates.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D4441
Base Resin Density 0.900 g/ccWeight of PTFE resin solids; ASTM D4441
Solids Content 60 %Percent of PTFE resin solids; ASTM D4441
Particle Size 0.22 µmAverage dispersion particle size
pH 9.5ASTM E70
Viscosity 20 cP
@Temperature 25.0 °C
ASTM D2196
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °CASTM D1457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Chemours Teflon® PTFE 8A Granular Molding Powder
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion
Chemours Teflon® PTFE Grade 305A Aqueous Dispersion

PDU9202 / 33321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.