MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUTENE FB0300 LDPE Blown Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the excellent mechanical properties and high stress cracking resistance make suitable for heavy duty bags and particularity bottom sealed bags. (LUTENE FB0300 contains no slip agent.)

Main Application: Packing of heavy products, Shrink hoods, Pallet shrink covers, all types of industrial packing

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.921 g/ccASTM D1505
Water Vapor Transmission 10.0 g/m²/day
Oxygen Transmission Rate 2000 cc/m²/day
Nitrogen Transmission 3500 cc-mm/m²-24hr-atm
Environmental Stress Crack Resistance >= 500 hourF50; ASTM D1693
Thickness 20.0 - 100 microns
 50.0 - 300 microns
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 550 %ASTM D882
Film Elongation at Break, TD 650 %ASTM D882
Tear Strength 370 kg(f)/cmMD; ASTM D1922
 380 kg(f)/cmTD; ASTM D1922
Dart Drop Test 300 gASTM D1709
Film Tensile Strength at Break, MD 23.5 MPaASTM D882
Film Tensile Strength at Break, TD 22.6 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 °CDSC
Crystallization Temperature 104 °CASTM D1525
Vicat Softening Point 95.0 °CASTM D1525
Brittleness Temperature <= -60.0 °CASTM D740
 
Optical PropertiesOriginal ValueComments
Haze 17 %ASTM D1003
Gloss 95 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 220 °C
Blow-up Ratio (BUR) 1.5 - 2.0
 
Descriptive Properties
Slip Coefficient0.47ASMT D1894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUTENE BB0808 LDPE Blown Film Grade
LG Chemical LUTENE FB0800 LDPE Blown Film
LG Chemical LUTENE CCO550BK PE Compound
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film

PLAY213 / 148223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.