AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural thin wall applications and where good glass distributions into features such as ribs and bosses is desired. Mechanical properties and mold shrinkage measured on flat plaques. Information provided by Azdel. |