MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silres® 601 Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: Flaked silicone resin containing phenyl groups and exhibiting good compatibility with organic resins.

Application: SILRES® 601 can be used for the following applications:

  • Base material for heat resistant powder coatings
  • Heat resistant coatings are formulated from heat resistant binders, heat resistant pigments and fillers.
  • For heat resistant powder coatings, SILRES® 601 is normally blended with standard organic powdercoating resins in a ratio of 1:1 to 2:1. Generally, incompatibilities are not expected.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 50.0 - 70.0 °C
 
Descriptive Properties
AppearanceFlakes
Colorcolorless to yellowish
Content (%)5OH group

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Glyptal 86009 Aluminum Pigmented Silicone Resin
NuSil CF2-4721 Silicone Resin
NuSil CF-4721 Silicone Resin
Parker Chomerics CHO-BOND® 1055, Part A Silicone Resin Mixture

PWACK9524 / 205053

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.