MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 58.4 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ASTM D2240
Tensile Strength, Yield 54.5 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 30 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2830 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 79.3 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 850 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 76.1 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 72.8 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
ALL; UL 94
 5VA
@Thickness 1.91 mm
ALL; UL 94
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %
@Thickness 3.81 mm
ASTM D1003
Transmission, Visible 78 %
@Thickness 3.81 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 204 °C
 
Descriptive Properties
Agency RatingsNSF 61
 NSF Unspecified Rating
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Impact Resistance
 Medium Flow
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFluid Handling
 General Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 83510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid

PH0POL0153 / 144722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.