MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller Hydra FAST-EN ™ DC-13239 Water-Based Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: Hydra FAST-EN TM DC-13239 is a water-borne two part sprayable adhesive designed to bond various substrates found in the marine industry. These include open cell urethane foams, foam-backed headliners, marine carpet, fiberglass (bare & gel coated), treated wood, aluminum, and various fabrics and plastics. The system is user-friendly and addresses many of the common problems encountered with other two part systems. Other applications where the use of solvent based, flammable and non-flammable systems are a concern for either health or environmental reasons may also be suitable candidates for the use of this product.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccPart A
 1.115 g/ccPart B
Solids Content 15 %Part B
 55 %
 55 %Part A
Volatile Organic Compounds (VOC) Content 0.46 g/lPart A
pH 3.5Part B
 12Part A
Viscosity <= 100 cPPart A, #2 @ 10 rpm
Storage Temperature 40.0 - 80.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 MonthPart A
 12.0 MonthPart B
 
Descriptive Properties
Base compoundPolychloroprenePart A
 Zinc SulfatePart B
ColorClearPart B
 White when wet (unless tinted)Part A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL119 / 316910

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.