MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PSI 825EX Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of thermoformed cups and containers. Other features include excellent extrusion processing, good gloss, and FDA compliance.

825EX is utilized in such products as drinking cups, dairy containers, bowls, and drink lids.

Information provided by Total Petrochemicals, Inc.

Key Words: High impact, high stiffness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4000 psiASTM D638
Elongation at Yield 45 %ASTM D638
Tensile Modulus 310000 psiASTM D638
Flexural Strength 8000 psiASTM D790
Flexural Modulus 360 ksiASTM D790
Izod Impact, Notched 1.90 ft-lb/inASTM D256
Falling Dart Impact 10.0 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FHeat Distortion, Annealed; ASTM D648
Vicat Softening Point 210 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 90 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSI 825 Polystyrene
Total PSI 825E Polystyrene
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
Total PSI 740 Polystyrene
Total PSC 1540(AS) Crystal Polystyrene

PFIM915 / 38320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.