MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex PTS-Creamid A3H2G5FRSE*800 Polyamide 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Form: Pellets

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation 3.8 %3.8 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiISO 527-2
Elongation at Break 3.7 %3.7 %ISO 527-2
Tensile Modulus 7.93 GPa1150 ksiISO 527-2
Flexural Strength 140 MPa20300 psiISO 178
Flexural Modulus 6.30 GPa914 ksiISO 178
Izod Impact, Notched (ISO) 9.03 kJ/m²4.30 ft-lb/in²ISO 180
Charpy Impact Unnotched 5.04 J/cm²24.0 ft-lb/in²ISO 179
Charpy Impact, Notched 0.903 J/cm²4.30 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75-2/A
Vicat Softening Point 240 °C464 °FISO 306/B
 250 °C482 °FISO 306/A
Flammability, UL94 V-0
@Thickness 0.787 mm
V-0
@Thickness 0.0310 in
Oxygen Index 30 %30 %ISO 4589-2
Glow Wire Ignition Temperature 799 °C
@Thickness 1.52 mm
1470 °F
@Thickness 0.0600 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.787 mm
1760 °F
@Thickness 0.0310 in
IEC 60695-2-12
 960 °C
@Thickness 1.52 mm
1760 °F
@Thickness 0.0600 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 °C554 °F
Melt Temperature 265 °C509 °FISO 11357-3
 280 - 295 °C536 - 563 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex PTS-Creamid A3H2G5FRSE*800 Polyamide 66, Dry
Teknor Apex PTS-Creamid A3H2G6FRSE*800 Polyamide 66, Dry
Teknor Apex PTS-Creamid A3H2G8.2FRS*9200 Polyamide 66 + PA 6I/6T, Dry
Teknor Apex Chemlon® A60XTH Polyamide 66

PTEKNQ0974 / 237465

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.