MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Rhodiacid™ Di Basic Acid DBA
Categories: Other Engineering Material

Material Notes: Product Description: DBA Di-Basic Acid is a mixture of aliphatic diacids (adipic, glutaric and succinic acids) including small quantities of nitric acid and metals

Market / Applications:

  • Water treatment
  • Solvent precursor
  • Leather Treatment
  • Desulphurization Agent
CAS No: 124-04-9, 110-94-1, 110-15-6, 7697-37-2

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH <= 1.0
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 40.0 °C
 
Descriptive Properties
AppearanceYellow liquid
Content10-40%Glutaric acid
 3-10%Nitric acid
 5-15%Succinic acid
 5-15%Adipic acid
Solubility in Water10 g/100ml

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Miracll G365 Bio-based Polyester TPU
Telles Bio-based Natural Plastics™ Aliphatic Copolyester, for Injection Molding
LATI Latigea B01 F1 Bio-Polymer
Lanxess BioAdimide® 100 Plastic Additive
Kaneka PHBH Rigid Bio-based Polymer

PSOLVAY677 / 218405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.