MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 4150H Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Normalized (heated to 870°C, air cooled)

AISI 4150 is notable for increased hardenability with a small tradeoff in machinability. Best strength and hardness appears in preheat-treated condition. Tailoring carbon content to bar size allows uniform physical attributes to be maintained across a variety of sizes.

Key Words: Chromium-molybdenum steels, UNS H41500, ASTM A304, SAE J1268, DIN 1.7228, JIS SCM 5, JIS SCM 5 H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 375
Hardness, Knoop 405Converted from Brinell
Hardness, Rockwell B 100Converted from Brinell
Hardness, Rockwell C 41Converted from Brinell
Hardness, Vickers 397Converted from Brinell
Tensile Strength, Ultimate 1340 MPa
Tensile Strength, Yield 896 MPa
Elongation at Break 10 %in 50 mm
Reduction of Area 24.8 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steels
Poissons Ratio 0.29Calculated
Machinability 55 %annealed and cold drawn; based on AISI 1212 as 100% machinability
Shear Modulus 80.0 GPaTypical for steels
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000245 ohm-cmTypical 4000 series steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical 4000 series steel
Thermal Conductivity 44.5 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.47 - 0.54 %
Chromium, Cr 0.75 - 1.2 %
Iron, Fe 96.535 - 97.83 %As remainder
Manganese, Mn 0.65 - 1.1 %
Molybdenum, Mo 0.15 - 0.25 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4150 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Assab Steels 709M Machinery Steel
AISI 4150H Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 4150H Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 4150 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round

M4150L / 7612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.