MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Röhm ACRYLITE® Film White WF002 PMMA
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: PLEXIGLAS® Film WF002 is a high weather resistant, glossy and white acrylic film for graphic printings and high quality laminations. Due to its excellent performance under long term weathering and UV light exposure, PLEXIGLAS® Film WF002 does not present color change or yellowing. Its glossy and very smooth surface leads the film to provide an excellent printing quality.

Application: PLEXIGLAS® Film WF002 can be used to be printed on as high quality film decoration and then laminated on different polymeric films and sheets. Laminated decoration films protected by PLEXIGLAS® are suitable for a wide range of molding processes such as thermoforming and insert molding. PLEXIGLAS® Film WF002 can be used as a single face layer in high UV and weathering resistant durable labels and tapes without the need for an overlay film.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³DIN 53479
Surface Tension 50 dynes/cm50 dynes/cmDIN 53364
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-3
Elongation at Break >= 50 %>= 50 %ISO 527-3
Elongation at Yield 5.0 %5.0 %ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 95.0 °C203 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polycasa Acryl® KR 2007/1 Acrylic

PEVONIL039 / 196243

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.