Hostacom XBR 169 G C12509 is a 16% talc filled PP copolymer, with high impact resistance and good scratch resistance. The product is also available as a customized color matched, pellet form. This grade is delivered in C12509 color version. Applications: Instrument PanelsInformation provided by LyondellBasell. |