MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GF 9045 F High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Hostalen GF 9045F is a high density Polyethylene, having medium molar mass and a narrow molecular mass distribution. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Products for Use in Property Modification

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccISO 1183-1
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.0 MPaISO 527-1,-2
Film Elongation at Break, MD 520 %ISO 527-1,-3
Tensile Modulus 900 MPaISO 527-1,-2
Dart Drop Test 45.0 gASTM D1709
Film Tensile Strength at Break, MD 60.0 MPaISO 527-1,-3
Film Tensile Strength at Break, TD 50.0 MPaISO 527-1,-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CPeak; ISO 11357-3
Vicat Softening Point 75.0 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 230 °C
 
Descriptive Properties
Processing MethodBlown Film
Test Specimenfilm, 30µm blown film extruded at 190°C and a blow up ratio 3:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications

PEQT8488 / 220123

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.