MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Water Absorption 0.18 %24 hours at 73°F; ASTM D570
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 55.0 MPa
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 86.0 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.07 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 14.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secPLC 6
Comparative Tracking Index 250 - 400 VPLC 2
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 1.50 mm
PLC 3
 30 - 60 sec
@Thickness 3.00 mm
PLC 2
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 3.00 mm
PLC 1
 >= 120 arcs
@Thickness 1.50 mm
PLC 0
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minPLC 3
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 39.0 µin/in-°F
@Temperature -40.0 - 95.0 °C
ASTM E831-06
CTE, linear, Transverse to Flow 38.0 µin/in-°F
@Temperature -40.0 - 95.0 °C
ASTM E831-06
Deflection Temperature at 0.46 MPa (66 psi) 135 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CASTM D648
 137 °CISO 75
UL RTI, Electrical 125 °C
UL RTI, Mechanical with Impact 115 °C
UL RTI, Mechanical without Impact 125 °C
Flammability, UL94 V-1
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
Oxygen Index 36.9 %ASTM D2863
Glow Wire Ignition Temperature 775 °C
Glow Wire Flammability Index 960 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 490 - 525 °F
Middle Barrel Temperature 510 - 530 °F
Front Barrel Temperature 530 - 560 °F
Nozzle Temperature 520 - 560 °F
Melt Temperature 540 - 580 °F
Mold Temperature 160 - 200 °F
Drying Temperature 250 °F
Dry Time 4 hour
Injection Pressure 11000 - 18000 psi
Back Pressure 50.0 - 200 psi
Clamp Pressure 4000 - 10000 psi
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow to Medium
Injection Speed- Tab GateMedium to Fast
Injection Speed- Tunnel GateFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release
Covestro Bayblend® T65 HG PC/ABS Blend
Lotte Advanced Materials Infino® HN-1064IA PC, Unreinforced FR
Overview of materials for Polycarbonate, UV Stabilized

PZ9PT91a / 21525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.