Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Additive: Plasticizer Features: Non-Phthalate Plasticizer; Radiation Sterilizable Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |