MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt HiGloss TR™ 99R Series High Performance Low VOC Gel Coat for Reinforced Plastics
Categories: Polymer; Thermoset

Material Notes: HiGloss TRTM 99R gel coats are high performance products formulated for the Reinforced Plastics Composites Industry.

Features and Benefits:

  • Resistant to water and certain chemicals
  • Provide durable, reduced maintenance products

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 3550 cPColor, RVF, spindle #4 @ 20 rpm
 4800 cPWhite, RVF, spindle #4 @ 20 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 88.0 °FWhite
 88.0 °FColor
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 45.0 minWhite, Lay-up Time
 15.0 - 45.0 minColor, Lay-up Time
Gel Time 15.0 min
@Temperature 25.0 °C
White, 100 g mass, 77 ºF with 1.8% MEK-Peroxide
 15.0 min
@Temperature 25.0 °C
Color, 100 g mass, 77 ºF with 1.8% MEK-Peroxide
 
Descriptive Properties
Sag ResistanceGood @ 20 milsWhite
 Good @ 20 milsColor
Thixotropic Index62/20 rpm, White
 62/20 rpm, Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9205 / 231800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.