MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil MED-6400 Dispersion - Unrestricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of various molecular weights and reinforcing fillers. The substituent groups comprising the polymer back bone structure may consist of the following: Polydimethylsiloxane, Dimethyl Diphenyl copolymer, and Fluoro homo polymer or copolymer. Silicone dispersions typically have low viscosities, which is beneficial for applications wherein a thin film coating is needed, and they can easily be used in dipping and spraying processes. NuSil uses a variety of solvents to disperse silicones, such as xylene, tert butyl acetate, heptane, hexane, acetone and naphtha.

Important Properties of Dispersions: Prior to curing, dispersions can exhibit various uncured properties, as listed below. These properties define the characteristics of dispersions and their behavior during application:

  • Addition or moisture cure
  • Supplied as one or two part system
  • Viscosity and Rheology - Most dispersions are shear thinning, meaning the viscosity decreases with increase in shear.
  • Viscosity decreases by decreasing the solids content
Comments: 1.43 RI in Xylene

Cure Systems: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
Viscosity 600 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 35Certified
 30Typical
Tensile Strength at Break 6.60 MPaCertified
 10.3 MPaTypical
Tensile Stress at Strain 350 psi
@Strain 300 %
Elongation at Break 600 %Certified
 775 %Typical
Tear Strength 130 pliCertified
 150 pliTypical
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 25.0 °C
+ 45m / 75°C + 135m / 150°C
Working Life 24.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Polyvinyl Fluoride (PVF) Film
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Dow AMS-C30 Cosmetic Wax

PNUSIL341 / 142065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.