MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem P-4000
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Applications: Zinc and calcium stearate provide lubricity, plasticizing and release properties in polymer systems. Stearates may be added internally into compounds or applied externally to uncured rubber slabs or extrusions. Zinc stearate can replace stearic acid and part of the zinc oxide in a compound and improve processing properties. As a process aid, calcium stearate aids EPDM extrusion smoothness and nitrile release from metal. Calcium stearate is often substituted for zinc stearate in those plants that must reduce zinc in water runoff. The higher melt point of the calcium stearates can be of advantage in high temperature processes. Zinc and calcium stearates have specific gravities of 1.095 and 1.035.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 325 Mesh325 Mesh0.995
Ash 10 %10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 2.5 %<= 2.5 %
 
Descriptive Properties
Content0.0015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH594 / 315512

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.