MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Germanium (Ge)
Categories: Pure Element

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.33 g/cc
@Temperature 25.0 °C
Solubility 0.00 ppm
a Lattice Constant 5.657 Å
Molecular Weight 72.61 g/mol
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 9000MPa
Hardness, Mohs 6.0
Modulus of Elasticity 103.2 GPain <100> direction
 155.6 GPain <111> direction
Poissons Ratio 0.278
Shear Modulus 46.7 GPain <111> direction
 67.2 GPain <100> direction
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.10 - 5.80 µm/m-°C
@Temperature -60.0 - 60.0 °C
Specific Heat Capacity 0.310 J/g-°C
Thermal Conductivity 59.8 W/m-K
@Temperature 27.0 °C
Melting Point 937 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 4.0034n10.6
 4.0017
@Wavelength 15000 nm
 4.004
@Wavelength 10000 nm
 4.0076
@Wavelength 7000 nm
 4.1079
@Wavelength 2000 nm
IR Transmittance 56 %
@Wavelength 15000 nm
Internal Transmittance
 70 %
@Wavelength 12000 nm
Internal Transmittance
 97 %
@Wavelength 3000 nm
Internal Transmittance
 97 %
@Wavelength 9000 nm
Internal Transmittance
 
Descriptive Properties
Cleavability(111)perfect
Constants of Elastic Compliance (Pa^-1)1.489E-11
 -2.65E-12
 9.69E-12
Symmetrycubic
Symmetry Classm3m
Thermal Coefficient of Refractive Index3.5E-4 to 4E-43.39 microns for ± 60°C
Transmission Range (microns)2 - 17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Germanium, Ge
Americium, Am
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked
Gold, Au

CMAT043 / 87727

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.