Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange Sealant Product has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dresses gaskets in rigid assemblies. Eliminates gasket compression set. Recommended Primer: 7649 (N). UL classified Typical Use: High temperature applications, Excellent solvent resistance |