MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Neutrex Purgex™ 3057 Plus Purging Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Blend, polyethylene, 3% glass, and FDA-approved active component. Non-toxic, non-abrasive and safe. Ready to use and easy to remove

PURGEX 3057 Plus thoroughly removes all types of colorants and engineering resins, such as nylon and polycarbonate, from the barrel, screw, and nozzle of thermoplastic resin injection molding, extrusion, or blow molding equipment, as well as hot runner systems. PURGEX 3057 Plus includes a modified polyethylene for higher temperature resins. PURGEX 3057 Plus can be used for rapid turnaround on color and material hanges with challenging resins such as LCP, PBT, and PPO, on alloys such as PC/ABS, and is recommended for glass- or mineral-filled applications. This blend operates up to 600°F (316°C) with a five minute soak, or higher temperatures without a soak.

Key Words: Purge
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 - 600 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chisso Z CLEAN® A1 Purging Solution
Celanese ZENITE 5244L LCP, 40% Mineral / Glass Reinforced
Avient PolyAdd™ 1922 Purge Compound

PNEUTR01 / 81839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.