MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY SC2052 PC+GF, Injection Molding
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Good Toughness, Good Impact, Good Surface

Application: Mobile Phone Housing

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 53.0 MPa
@Thickness 3.20 mm
7680 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 90.2 MPa
@Thickness 3.20 mm
13100 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.65 GPa
@Thickness 3.20 mm
384 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched 4.41 J/cm8.27 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 275 - 290 °C527 - 554 °F
Middle Barrel Temperature 285 - 305 °C545 - 581 °F
Front Barrel Temperature 290 - 310 °C554 - 590 °F
Nozzle Temperature 285 - 300 °C545 - 572 °F
Melt Temperature 290 - 310 °C554 - 590 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C
@Time 10800 - 18000 sec
212 - 248 °F
@Time 3.00 - 5.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.981 - 3.92 MPa142 - 569 psi
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY SP2053 PC+GF, Injection Molding
Röchling SUSTANT® PC GF 20
Star Plastics PCGF30 Molding Grade PC with 30% Glass
Star Plastics PCGF20 Molding Grade PC with 20% Glass
Star Plastics PCGF10 Molding Grade PC with 10% Glass

PLHCHEM9702 / 239227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.