MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones SilPruf NB SCS9000 Non-staining Silicone Weatherproofing Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: GE SCS9000 SilPruf NB is a 100% silicone polymer sealant formulated to reduce or eliminate dirt pickup, surface streaking, and substrate staining. SCS9000 is a premium one-component, medium-modulus, neutral cure silicone sealant useful on a wide variety of materials in new or remedial applications. Supplied as a paste, SCS9000 produces a durable silicone rubber joint sealant upon cure.

Features: Silicone Durability, Adhesion, Movement Capacity, Low VOC Content, Thermal Stability (cured state). Application: • Stable Consistency (uncured state), Extended Work Life, Low Sag or Slump.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 37 g/lUncured; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 27ASTM D2240
Tensile Strength, Ultimate 1.68 MPaASTM D412
Elongation, Ultimate 629 %ASTM D412
Tear Strength 5.50 kg(f)/cmDie B.; ASTM D624
Peel Strength 36.8 pliASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 - 72.0 hour
 240 - 336 hourFull Cure
Tack-Free Time 60.0 - 120 min
@Temperature 22.8 °C
50% RH; ASTM C679
Working Life 30.0 - 40.0 min
 
Descriptive Properties
AppearancePaste
ColorAluminum GraySCS2900.09
 BlackSCS2900.03
 BronzeSCS2900.97
 Dark GraySCS2900.10
 Light GraySCS2900.08
 LimestoneSCS2900.04
 Precast WhiteSCS2900.20
 WhiteSCS2900.02
Consistency / Sag0.1” max
Joint Movement Capability±50%ASTM C719.
Silicone Content (%)100Uncured
Staining (Masonry)NoneCured. ASTM C1248.
UV & Weathering ResistanceExcellentGE 20 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9929 / 265740

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.