MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach Formadur® 2311 (P-20 MOD.) Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Formadur® 2311 is a pre-hardened plastic mold steel

Characteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231

Applications: Injection molds, Compression molds, Blow mold, Mold bases and Die holder

Information provided by Schmolz + Bickenbach

Key Words: AISI P-20
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 28
@Treatment Temp. 700.0 °C,
Time 7200 sec
 36
@Treatment Temp. 600.0 °C,
Time 7200 sec
 42
@Treatment Temp. 500 °C,
Time 7200 sec
 46
@Treatment Temp. 400 °C,
Time 7200 sec
 48
@Treatment Temp. 300 °C,
Time 7200 sec
 50
@Treatment Temp. 200 °C,
Time 7200 sec
 51
@Treatment Temp. 100 °C,
Time 7200 sec
Tensile Strength 134 ksi32 HRC
 123 ksi
@Treatment Temp. 700.0 °C
28 HRC
 165 ksi
@Treatment Temp. 600.0 °C
36 HRC
 193 ksi
@Treatment Temp. 500 °C
42 HRC
 215 ksi
@Treatment Temp. 400 °C
46 HRC
 228 ksi
@Treatment Temp. 300 °C
48 HRC
 242 ksi
@Treatment Temp. 200 °C
50 HRC
 251 ksi
@Treatment Temp. 100 °C
51 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.80 µin/in-°F
@Temperature 21.1 - 93.3 °C
 7.20 µin/in-°F
@Temperature 21.1 - 204 °C
 7.40 µin/in-°F
@Temperature 21.1 - 302 °C
Thermal Conductivity 221 BTU-in/hr-ft²-°F
@Temperature 302 °C
 233 BTU-in/hr-ft²-°F
@Temperature 204 °C
 235 BTU-in/hr-ft²-°F
@Temperature 100 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1310 - 1365 °FCooling: Furnace; < 235 HB
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 1.9 %
Iron, Fe 96 %
Manganese, Mn 1.5 %
Molybdenum, Mo 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Overview of materials for Mold Steel
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel

NSCHMO001 / 125874

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.