MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® 455 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 455 is a high clarity polyester film pretreated on one side for slip. It has excellent handling characteristics.

General Product Info:

  • Two smooth coatable surfaces
  • Low surface resistivity
  • Can be topcoated on either side
  • Improves safety and cleanliness
Approvals: Library of Congress Specification - This film meets the Library of Congress Specification Number 500-500-5/31/95 for use in archival storage.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 14000 psiASTM D882A
Film Tensile Strength at Yield, TD 14000 psiASTM D882A
Film Elongation at Break, MD 150 %ASTM D882A
Film Elongation at Break, TD 100 %ASTM D882A
Coefficient of Friction, Dynamic 0.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 36000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 87 %
@Thickness 0.165 mm
TLT; ASTM D1003
 88 %
@Thickness 0.118 mm
TLT; ASTM D1003
 88.3 %
@Thickness 0.0940 mm
TLT; ASTM D1003
 88.5 %
@Thickness 0.0686 mm
TLT; ASTM D1003
 88.7 %
@Thickness 0.0508 mm
TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 461 Polyester Film
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 457 Polyester Film, 200 Gauge

PDTZ9100 / 139488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.