MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Plastron® PA9T-CF30-01(L9) Long carbon fiber reinforced aromatic PA resin
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Long carbon fiber reinforced aromatic PA resin (GF30%)

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³Dry; ISO 1183
Filler Content 30 %30 %Carbon fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 350 MPa50800 psiDry; ISO 527-1,2
Flexural Strength 490 MPa71100 psiDry; ISO 178
Flexural Modulus 22.5 GPa3260 ksiDry; ISO 178
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 295 °C563 °FDry; ISO 75-1,2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 320 °C554 - 608 °F
Middle Barrel Temperature 300 - 330 °C572 - 626 °F
Front Barrel Temperature 310 - 340 °C590 - 644 °F
Nozzle Temperature 310 - 340 °C590 - 644 °F
Mold Temperature 140 - 160 °C284 - 320 °F
Drying Temperature 120 - 140 °C
@Time 18000 - 86400 sec
248 - 284 °F
@Time 5.00 - 24.0 hour
Back Pressure 1.00 - 5.00 MPa145 - 725 psi
Screw Speed 40 - 60 rpm40 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9929 / 305602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.