MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes:

Information provided by Niche Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.0080 - 0.012 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4100 psiASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 5200 psiASTM D790
Flexural Modulus 240000 psiASTM D790
Izod Impact, Unnotched 1.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 300 - 340 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 140 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman TPP20AJ36BK 20% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural
Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled
A. Schulman TPP20AF01HB 20% Talc-Filled Homopolymer Polypropylene
Avient Maxxam™ PD 20 TF Black Polypropylene

PNICHE025 / 178260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.