The Petrothene GA501 series of resins is pelletized liner low density polyethylene selected for film extrusion applications that require excellent drawdown and toughness. These resins have excellent puncture resistance, elongation and heat seal strength. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. GA501 is available without additives or fully formulated with slip and antiblock additives. GA501150 is formulated without TNPP. Applications: Agriculture Film, Bags & Pouches, Can Liners, Film Wrap, Food Packaging Film, Heavy Duty Packaging, Lamination Film, Liner Film, Retail Carryout Bags, Shrink FilmInformation provided by LyondellBasell. |