MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin; Epoxy Encapsulant, Unreinforced

Material Notes: Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and adhesion to most surfaces and is free flowing to penetrate voids and give good air release and a smooth high gloss surface. It has very good resistance to water, acids and bases and most organic solvents. It was especially formulated to a 2A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. EP691 will reach full cure at room temperature within 24 hours. Cure time can be accelerated by the application of heat after product has gelled. Times and temperatures from 1 hour at 65°C to 20 minutes at 100°C are typical for small castings (less than 50 grams).

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccPart B; TM R050-16
 1.11 g/ccMixed; TM R050-16
 1.16 g/ccPart A; TM R050-16
Water Absorption 0.17 %
@Time 86400 sec
TM R050-35
Viscosity 2500 cPPart B, RVT, #2, 20 rpm; TM R050-12
 9000 cPMixed; TM R050-12
 16000 cPPart A, RVT, #6, 20 rpm; TM R050-12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80TM R050-17
Tensile Strength at Break 7500 psiTM R050-36
Tensile Strength, Ultimate 8500 psiTM R050-36
Tensile Strength, Yield 7000 psiTM R050-36
Elongation at Break 4.0 - 9.0 %TM R050-36
Tensile Modulus 400 ksiTM R050-36
Compressive Yield Strength 11500 psiTM R050-38
Compressive Strength 25000 psiUltimate; TM R050-38
 25000 psiBreak; TM R050-38
Compressive Modulus 420 ksiTM R050-38
Adhesive Bond Strength 2000 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 410 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°C
Thermal Conductivity 0.140 W/m-K
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 80.0 °CTM R050-25
 
Processing PropertiesOriginal ValueComments
Pot Life >= 120 minMass: 50g; TM R050-19
 
Descriptive Properties
ColorLight Amber
Mix Ratio100:45Weight
 2:1Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Circalok™ 6037 Epoxy Adhesive

PRESL150 / 101564

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.