MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Nylon 6.6 for injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Water Absorption 1.5 - 2.2 %1.5 - 2.2 %ISO 62
Water Absorption at Saturation 6.0 - 8.0 %6.0 - 8.0 %ISO 62
Viscosity Measurement 145145Viscosity index; ISO 307
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm0.0080 - 0.020 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 140 MPa20300 psiISO 2039-1
Tensile Strength at Break 105 MPa15200 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 4.70 GPa682 ksiISO 527
Flexural Modulus 4.10 GPa595 ksiISO 178
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²DIN 53453
 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eU
 2.50 J/cm²
@Temperature -40.0 °C
11.9 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 3.20 J/cm²
@Temperature -30.0 °C
15.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 0.600 J/cm²2.86 ft-lb/in²DIN 53453
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V550 VCTI 100; IEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 3146 DSC
Maximum Service Temperature, Air 110 °C230 °FContinuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Envalior Akulon® S223-G2U PA66-GF13, Dry, 13% Glass Filled
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
BASF Ultramid® A34 01 PA66 (Dry)

PFRI089 / 39010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.