MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kohesi Bond KB 1040 LP - FRV Two component, flame retardant epoxy for aircraft interior applications
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Can pass FAR Standard 14 CFR 25.853 (a)
  • Capable of passing vertical burn test
  • Non-halogen filler
  • Excellent flow properties / can spray paint
  • Color matched to Pantone® Cool Gray 4 C
  • Extremely low smoke generation
Kohesi Bond KB 1040 LP - FRV is a two component, flame retardant, room temperature curing epoxy system suitable for coating, bonding, sealing, potting and encapsulation. It has a 100:30 (Part A: Part B) mix ratio by weight. This flame retardant epoxy is capable of passing the vertical burn test specifications as per Amendment 25-116 and Part 25 Appendix F of the FAR standards. It contains a non-halogenated filler, making it easy to handle and environmentally friendly. The optimum cure schedule for KB 1040 LP - FRV would be an overnight room temperature set-up followed by an addition of heat at 90°C for 3 - 5 hours. KB 1040 LP - FRV offers an extensive service temperature range of -51°C to +121°C. This product’s excellent flow properties and long working time makes it ideal for use in spray coating and casting applications. It offers excellent electrical insulation and excellent chemical resistance to a variety of fuels, oils, common solvents and water. Part A has a gray color and Part B has a white color. Upon mixing, it matches the Pantone® Cool Gray 4 C shade - commonly used for aircraft interiors. KB 1040 LP - FRV’s properties makes it ideal for use in aerospace and aviation related applications, such as door and floor assemblies, interior panels, food trays and electronic potting and sealing.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³Part B
 1.31 g/cc0.0473 lb/in³Part A
Viscosity 500 - 2000 cP500 - 2000 cPPart B
 2000 - 6000 cP2000 - 6000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength >= 66.2 MPa>= 9600 psi
Tensile Modulus 2.48 - 2.83 GPa360 - 410 ksi
Adhesive Bond Strength >= 19.3 MPa>= 2800 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.61
@Frequency 60 Hz
3.61
@Frequency 60 Hz
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Option 2
 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
Option 1
Working Life 60.0 - 90.0 min60.0 - 90.0 min100 g of mixed epoxy
Shelf Life 6.00 Month6.00 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI915 / 249094

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.