MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Palatinol® N Diisononyl Phthalate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Formula: C28H42O4

Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl compounds provides good low temperature and low volatility performance. It has excellent rheological properties in plastisols and offers improved dry blend times. The mechanical properties of vinyl compounds plasticized with Palatinol N are comparable to products plasticized with other diisononyl phthalates. The unique nature of this ester results in lower volatility, improved processibility and better low temperature performance.

Applications: The excellent resistance to water and outdoor exposure by vinyl plasticized with Palatinol N is an advantage in the manufacture of articles for the housing and construction markets. By virtue of its contribution to low viscosity and good viscosity stability, Palatinol N is suitable for plastisols including: spray coating, dipping, casting and slush molding.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 - 0.976 g/cc0.0350 - 0.0353 lb/in³ASTM D4052
Solubility of Water 0.0020 %0.0020 %
Solubility in Water <= 1.0e-6 %<= 1.0e-6 %
Viscosity  28 cP
@Temperature 40.0 °C
28 cP
@Temperature 104 °F
Absolute
 79 cP
@Temperature 20.0 °C
79 cP
@Temperature 68.0 °F
Absolute
 345 cP
@Temperature 0.000 °C
345 cP
@Temperature 32.0 °F
Absolute
Molecular Weight 418 g/mol418 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.070<= 0.070[mg KOH/g]; ASTM D1045
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  69
@Time 15.0 sec
69
@Time 0.00417 hour
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
 82
@Time 15.0 sec
82
@Time 0.00417 hour
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
 89
@Time 15.0 sec
89
@Time 0.00417 hour
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 13.0 MPa1890 psiPlasticizer conc. in vinyl film 70 phr; ASTM D638
 16.6 MPa2410 psiPlasticizer conc. in vinyl film 50 phr; ASTM D638
 17.8 MPa2580 psiPlasticizer conc. in vinyl film 40 phr; ASTM D638
Elongation at Break 280 %280 %Plasticizer conc. in vinyl film 40 phr; ASTM D638
 310 %310 %Plasticizer conc. in vinyl film 50 phr; ASTM D638
 350 %350 %Plasticizer conc. in vinyl film 70 phr; ASTM D638
100% Modulus  10.1 MPa
@Strain 100 %
1470 psi
@Strain 100 %
Plasticizer conc. in vinyl film 50 phr; ASTM D638
 14.10 MPa
@Strain 100 %
2045 psi
@Strain 100 %
Plasticizer conc. in vinyl film 40 phr; ASTM D638
 61.0 MPa
@Strain 100 %
8850 psi
@Strain 100 %
Plasticizer conc. in vinyl film 70 phr; ASTM D638
Torsional Stiffness  310 MPa
@Temperature -9.00 °C
45000 psi
@Temperature 15.8 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
 310 MPa
@Temperature -22.0 °C
45000 psi
@Temperature -7.60 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
 310 MPa
@Temperature -38.0 °C
45000 psi
@Temperature -36.4 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
 
Thermal PropertiesMetricEnglishComments
CTE, linear 700 µm/m-°C389 µin/in-°F
Boiling Point 252 °C
@Pressure 600000 MPa
486 °F
@Pressure 8.70e+7 psi
Pour Point -49.0 °C-56.2 °F
Brittleness Temperature -42.0 °C-43.6 °FPlasticizer conc. in vinyl film 70 phr; ASTM D746
 -31.0 °C-23.8 °FPlasticizer conc. in vinyl film 50 phr; ASTM D746
 -23.0 °C-9.40 °FPlasticizer conc. in vinyl film 40 phr; ASTM D746
Flash Point 240 °C464 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4861.486
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.10 %0.10 %ASTM E203
 
Descriptive Properties
Color<25APAH, ASTM D5386
CompositionEster content>99.6%, ASTM D3465

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Synplast™ TINTM-E Triisononyl Trimellitate
Silberline Silvex® 410-15-D
The Chemical Company VESTINOL® 9 Diisononyl Phthalate, C6H4(COOC9H19)2

PBASG0743 / 132376

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.