A single component static dissipative silicone/acrylic coating which provides excellent anti static protection in addition to its anti-corrosion properties. Continuous heat resistance is provided up to 350°C. Used in areas where ESD (electro static discharge) is to be avoided. Typical applications would include oven interiors, flow solder machines etc.Information provided by TBA Protective Solutions |