Scotch® Tape 897 is a glass-filament-reinforced tape suitable for light to medium duty strapping, bundling, reinforced applications. Scotch® Tape 897 has a synthetic rubber resin adhesive with good adhesion to most fiberboard surfaces and to a variety of plastic and metal surfaces.Information provided by 3M |