Selenis Bondz BO 144 is a copolyester specifically designed for sealing layers in BOPET films and delivers an extremely slow rate of crystallization. Selenis has developed this bonding solution to consistently deliver excellent melt strength and exceptional heat-sealing performance. This product is formulated to provide and sustain the adhesion level crucial to the packaging integrity through the different processes of manufacturing, securing full protection of the final product. Selenis Bondz BO 144 greatly improves converting steps, such as laminating, metalizing and printing. Selenis Bondz BO 144 is an amorphous copolyester resin dedicated to twin-screw extrusion. When using this kind of equipment, no drying is required prior to extrusion.Information provided by Selenis. |