MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SMAC CABLE® 2526S-20-08 Damping Material
Categories: Other Engineering Material

Material Notes: The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment.

Descriptions
Bars: Aluminum alloy
Screws: Inox A2
Threaded insert: Stainless steel
Standard treatment: SurTec 650

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 - 300 °C
 
Descriptive Properties
Damping Factor0.1 - 0.2
F, Max Dynamic13580 daN53.0 mm, up
 2925 daN155.0 mm, 45° down and out
 4280 daN95.0 mm, left and right
 4390 daN86.0 mm, up and down
 4860 daN105.0 mm, down
F, Max Static1215 daN35.0 mm, 45° down and out
 1620 daN20.0 mm, down
 1620 daN13.5 mm, up
 810.0 daN34.1 mm, up and down
 810.0 daN36.0 mm, left and right
Transmissibility at resonance3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Alodine T 5900 Conversion Coating
Henkel Alodine T 5900 RTU Conversion Coating
Henkel Alodine T 5923 Conversion Coating
Henkel Frekote 44-NC Mold Release Agent
Tricalcium-Phosphate (TCP), CA3(PO4)2

PZSMAC087 / 146203

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.