MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Xencor™ PPA LGF-1930 HS Long Glass Fiber Thermoplastic
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: Long Glass Fiber Thermoplastic. PPA base, 30% LGF. Heat stabilized. Natural.

Xencor™ PPA LGF-1930 HS is a 30% Long Glass Fiber reinforced, heat stabilized polyphthalamide PPA, with high heat deflection temperature, very high flexural modulus and low moisture absorption. It displays an excellent retention of properties in a wide temperature range as well as outstanding creep and fatigue resistance.

Xencor™ PPA LGF-1930 HS has a pellet length of 9mm and can be processed on most injection-molding machines.

- Black: Xencor™ PPA LGF-1930 HS BK 545-9
- Natural: Xencor™ PPA LGF-1930 HS NT-9

Applications: Aircraft Applications; Automotive Applications; Consumer Applications; Industrial Applications

Features: Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Temperature Stiffness; Low CLTE; Low Shrinkage; Low Warpage

Injection notes: Pre-Drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried.
Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 20% and only regrind of optimum quality should be used. In any case, part properties should be checked.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa
@Temperature 120 °C
ISO 527-2
 160 MPa
@Temperature 90.0 °C
ISO 527-2
 180 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 6500 MPa
@Temperature 120 °C
ISO 527-2
 10000 MPa
@Temperature 90.0 °C
ISO 527-2
 11000 MPa
@Temperature 23.0 °C
ISO 527-2
Flexural Strength 275 MPaISO 178
Flexural Modulus 10300 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²ISO 179
Charpy Impact, Notched 20.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 300 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 285 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 330 - 340 °C
Middle Barrel Temperature 340 °C
Front Barrel Temperature 340 °C
Nozzle Temperature 335 - 345 °C
Melt Temperature <= 345 °CInjection
Mold Temperature 135 - 160 °C
Drying Temperature 120 °C
@Time 14400 - 28800 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingCompression Molding; Injection Molding; Overmolding
RoHS ComplianceYes
Suggested Max Regrind (%)20Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4630 / 280430

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.