MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.

Nylon 6 with 50% carbon fiber reinforcement

Information provided by PlastiComp, Inc.

Key Words: Complet® Long Fiber LCF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D-792
Filler Content 50 %Carbon Fiber
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 310 MPaASTM D-638
Elongation at Break 1.0 %ASTM D-638
Tensile Modulus 37241 MPaASTM D-638
Flexural Strength 503 MPaASTM D-790
Flexural Modulus 28276 MPaASTM D-790
Izod Impact, Notched 240 J/mASTM D-256
Izod Impact, Unnotched 961 J/mASTM D-4812
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 530 °F
Middle Barrel Temperature 510 - 540 °F
Front Barrel Temperature 520 - 550 °F
Nozzle Temperature 520 - 550 °F
Melt Temperature 520 - 550 °F
Mold Temperature 200 °F
Injection Velocity 2.00 - 3.00 in/sec
Drying Temperature 85.0 °C
@Time 14400 sec
Moisture Content <= 0.18 %
Back Pressure 25.0 - 50.0 psi
Cushion 0.250 in
Screw Speed 30 - 50 rpm
 
Descriptive Properties
Injection PressureMedium to maximum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlisle 201LD Carbon-Carbon Composite
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black
Overview of materials for Nylon 6, Unreinforced
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced

PPLASTI927 / 159580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.